Polymer Property : Film Tensile Strength at Break, TD = 2.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 2.10 - 28.8 MPa
305 - 4180 psi
Average value: 20.3 MPa Grade Count:6
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Film Tensile Strength at Break, TD 2.10 MPa
305 psi
ASTM D882
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s..