Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 20.4 MPa
2960 psi
ASTM D882
ExxonMobil LD 316.19 High Clarity, High Impact Film Resin
LD 316.19 has improved impact strength and heat sealability versus homopolymer clarity film resins. Applications include frozen and other food packaging, as well as profile extrusion.Information pr..