Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
Chevron Phillips 6109FK Linear low density polyethylene blown film resin
(discontinued **) Resin Type: linear low density polyethylene, butene copolymer, medium antiblock, medium slip, process aid version of 6109, blown film resinCharacteristics: good stiffness at thin gauges, good drawdo.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
LyondellBasell Plexar® PX2049 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
(discontinued **) General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer
(discontinued **) Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177.. |
|||
Film Tensile Strength at Break, TD | 21.4 - 39.3 MPa | 3100 - 5700 psi | ASTM D882 |
Honeywell PMP Polymethylpentene Film
(discontinued **) PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
LyondellBasell Petrothene® NA340141 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
LyondellBasell Petrothene® NA340163 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
LyondellBasell Petrothene® NA340185 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
LyondellBasell Petrothene® NA340212 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
LyondellBasell Petrothene® NA340013 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
Westlake EF1807 Low Density Polyethylene Westlake Polyethylene EF1807 is a low density formulation suggested for film applications that require toughness.Application/UsesShrink filmFrozen food packagingFDA: This material complies with FDA .. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
Westlake EN1807AA Low Density Polyethylene WESTLAKE polyethylene EN1807 is a fractional-melt low- density formulation suggested for film applications requiring high impact strength, high tear strength, and very good optical properties, such .. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
Westlake LF1040 Butene Linear Low Density Polyethylene Westlake LF1040 is a butene LLDPE resin with excellent mechanical and sealing properties. It can be used in stretch film and can liner applications, and is suitable for blending with LDPE in packagi.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
Westlake LF1050 Butene Linear Low Density Polyethylene Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
ExxonMobil LDPE LD 105.30 Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Break, TD | 21.4 MPa | 3100 psi | ASTM D882 |
M. Holland Company MAGMA® LL1092-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |