Film Tensile Strength at Break, TD 216 MPa
31300 psi
ASTM D882A
DuPont Teijin Films Melinex® 238 Polyester Film
Melinex® 238 is a translucent white polyester film used for electrical insulation. It has been specially developed for use as an electrical insulation material in rotating electrical machines. It i..
Film Tensile Strength at Break, TD 216 MPa
31300 psi
ASTM D882A
DuPont Teijin Films Melinex® 618 Polyester Film, 700 Gauge
Melinex® 618 is a super clear polyester film, pretreated on one side to promote adhesion. It is a high clarity, non-yellow base with excellent adhesion on the pretreated surface. Used for a wide ra..