Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 16.1 MPa | 2330 psi | ASTM D3759 |
3M Scotch® 3771 Standard Message Box Sealing Tape Scotch® Box Sealing Tape 3771 is a standard message packaging tape used for box sealing, splicing, recouperage and other packaging applications. This product has a conformable backing and a consist.. |
|||
Film Tensile Strength at Break, TD | 16.1 MPa | 2330 psi | ASTM D3759 |
3M Scotch® 3779 Security Message Box Sealing Tape Scotch® Security Message Box Sealing Tape 3779 is an industrial packaging tape used for box sealing specifically where security of the carton contents is a concern. The printed design along with th.. |
|||
Film Tensile Strength at Break, TD | 16.1 MPa | 2330 psi | ASTM D3759 |
3M Scotch® 371 Industrial Box Sealing Tape Scotch® Box Sealing Tape 371 is an industrial packaging tape used for box sealing, splicing, recouperage and other packaging applications. This product has a conformable backing and a consistent pr.. |
|||
Film Tensile Strength at Break, TD | 16.1 MPa | 2330 psi | ASTM D3759 |
3M Scotch® 3781 Industrial Continuous Taping System Tape Scotch® Taping System Tape 3781 is an industrial continuous packaging tape used for box sealing and specially designed for use with the 3M-Matic™ Continuous Taping System (CTS) stand. The Product .. |
|||
Film Tensile Strength at Break, TD | 16.1 MPa | 2330 psi | ASTM D882 |
Westlake EMAC® SP2261 23% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2261 is a 23% EMA copolymer containing antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal tempe.. |