Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 24.3 MPa | 3520 psi | ASTM D882 |
ExxonMobil LL 1235x70 Cast Film Resin
(discontinued **) LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 24.3 MPa | 3530 psi | ASTM D882 |
ExxonMobil LD 051.LJ Shrink Film Resin
(discontinued **) LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr.. |
|||
Film Tensile Strength at Break, TD | 24.3 MPa | 3530 psi | ASTM D882 |
ExxonMobil LD 051.LT Shrink Film Resin
(discontinued **) LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr.. |