Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 24.5 MPa
3550 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF2021 Linear low density polyethylene resin  (discontinued **)
LF2021 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown and cast film extrusion which offers outstandin..
Film Tensile Strength at Break, TD 24.5 MPa
3550 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF2024 Linear low density polyethylene resin  (discontinued **)
LF2024 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and ..
Film Tensile Strength at Break, TD 24.5 MPa
3550 psi
500mm/min, Ultimate; ASTM D638
LG Chemical SEETEC BF315 LDPE
Characteristics: Good Processability and Excellent Optical PropertiesApplications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical
Film Tensile Strength at Break, TD 24.5 MPa
3550 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene
LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
Film Tensile Strength at Break, TD 24.5 - 38.2 MPa
3550 - 5540 psi
Average value: 31.0 MPa Grade Count:7
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..
Film Tensile Strength at Break, TD 24.5 MPa
3550 psi
Kuraray HYBRAR® BF1 Three Layer Blown Film
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber w..