Polymer Property : Film Tensile Strength at Break, TD = 245 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 35MB666 OPP Film
Product Description: A is a biaxially oriented transparent polypropylene film, acrylic coated tow sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle E..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 40MB666 OPP Film
Product Description: A is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle Ea..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 40MB668 OPP Film
Product Description: A high speed transparent biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides excellent perfo..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 42MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent PP film, coated one side PVdC, one side acrylic, This film provides outstanding performance on all packaging machines.Availabi..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 52MBR666 OPP Film
Product Description: Bicor 52MBR666 is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high mo..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 35LL666 OPP Film
Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 40LL666 OPP Film
Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 50LGT702 OPP Film
Product Description: A transparent biaxially oriented polypropylene film coated one side resistant coating and one side with a specially formulated acrylic coating. This film is designed for cut and..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 50LL210 OPP Film
Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 50LL539 OPP Film
Product Description: A clear, two-side coated, polypropylene label face stock designed for demanding pressure sensitive applications where outstanding ink adhesion and adhesive anchorage are require..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 50LL539 OPP Film
Product Description: A clear, two-side treated, polypropylene label facestock designed for demanding pressure sensitive applications where outstanding ink adhesion and adhesive anchorage are require..
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 57LL210 OPP Film
Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur..