Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 251 MPa | 36400 psi | 510 |
ExxonMobil Hicor® 110 BIHD-ASB OHD Film One-side acrylic, one-side PVdC coated, oriented high density polyethylene film. This film provides tack seal capability and excellent deadfold. Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 251 MPa | 36400 psi | 510 |
ExxonMobil Hicor® 90 BIHD OHD Film Clear, non-sealable, oriented high density polyethylene film. The surfaces have been modified for optimum machine performance in twistwrap applications. One side is treated for printing and laminati.. |
|||
Film Tensile Strength at Break, TD | 251 MPa | 36400 psi | 510 |
ExxonMobil Hicor® 90 BIHD-M OHD Film Metallized, non-sealable, oriented high density polyethylene film. The inside surface has been modified for optimum machine performance in twistwrap applications.Information provided by ExxonMobil C.. |