Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 175 MPa
25400 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 52LLC210 Preliminary Data Sheet OPP Film
Product Description: A clear gloss, surface-printable polyolefin film with enhanced conformability and squeezability for use in face-stock pressure sensitive applications. The proprietary core const..