Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 275 MPa | 39900 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 25MB866 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side PVOH. It provides excellent gas and aroma protection and is designed to be use.. |
|||
Film Tensile Strength at Break, TD | 275 MPa | 39900 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 26MB768 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VLTS) coating. PVdC provides an excellent moi.. |
|||
Film Tensile Strength at Break, TD | 275 MPa | 39900 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 30MB666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Film Tensile Strength at Break, TD | 275 MPa | 39900 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 30MBR666 OPP Film Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist.. |
|||
Film Tensile Strength at Break, TD | 275 MPa | 39900 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 32MB768 OPP Film Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu.. |
|||
Film Tensile Strength at Break, TD | 275 MPa | 39900 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL666 OPP Film Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |