Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 18 µm) HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 25 µm) HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 30 µm) HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 20 µm) HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 20 µm) HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 25 µm) HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 30 µm) HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 18 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 30 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 20 µm) HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead HSS13 Normal Grade Heat Sealable Film (thickness: 18 µm) HSS13 is a metalizing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has coron.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead PL11 Lamination Grade BOPP Plain Film (thickness: 12 µm) PL11 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminating.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead PL11 Lamination Grade BOPP Plain Film (thickness: 15 µm) PL11 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminating.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead PL13 Lamination Grade BOPP Plain Film (thickness: 15 µm) PL13 is a woven bag lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminatin.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead PL13 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL13 is a woven bag lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminatin.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead PL21 Lamination Grade BOPP Plain Film (thickness: 12 µm) PL21 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. It has excellent dimensional stability, high tensile strength,.. |
|||
Film Tensile Strength at Break, TD | 280 MPa | 40600 psi | ASTM-D882 |
Kinlead PL21 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL21 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. It has excellent dimensional stability, high tensile strength,.. |