Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 0.0248 - 0.0345 MPa | 3.60 - 5.00 psi | ASTM D882 |
BiologiQ ESR-PE EcoStarch mLLDPE Blend Properties of 70% mLLDPE, 25% ESR, 5% additive blend - thin filmInformation provided by BiologiQ |
|||
Film Tensile Strength at Break, TD | 0.0248 - 55.1 MPa | 3.60 - 7990 psi | Average value: 33.1 MPa Grade Count:244 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |