Film Tensile Strength at Break, TD 30.2 MPa
4380 psi
Calculated from mfr's report of 116 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® E56 Paper, 15 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..