Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 22.4 MPa
3250 psi
ASTM D882
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin
LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 22.4 MPa
3250 psi
ASTM D882
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin
LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical