Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 38.61 MPa
5600 psi
ASTM D882
ExxonMobil HD 7925.30 Barrier Film Resin
Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A..