Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 274 MPa | 39700 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® HB3 Polyester Film, 100 Gauge Teijin® Tetoron® HB3 is a super smooth polyester film with a UV absorbing agent, originally designed for green house applications. It has excellent weather-durability, low color and low haze. It i.. |