Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 42.6 MPa | 6180 psi | ASTM D882 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |