Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, TD = 43500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 25 µm)
PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 30 µm)
PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 40 µm)
PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 50 µm)
PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 25 µm)
PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 30 µm)
PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 40 µm)
PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 50 µm)
PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 25 µm)
PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 30 µm)
PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 40 µm)
PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 50 µm)
PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 25 µm)
PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 30 µm)
PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 40 µm)
PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 50 µm)
PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 18 µm)
PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 20 µm)
PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 30 µm)
PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 40 µm)
PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I..
Film Tensile Strength at Break, TD 300 MPa
43500 psi
ASTM-D882
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 60 µm)
PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh..
Copyright © lookpolymers.com All Rights Reserved