Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 44.1 MPa
6400 psi
ASTM D882
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Film Tensile Strength at Break, TD 44.1 - 57.9 MPa
6400 - 8400 psi
ASTM D882
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Film Tensile Strength at Break, TD 44.1 MPa
6400 psi
ASTM D882
Lotte Chemical Titan TITANEX® HF0961 High density polyethylene Hexene-1 resin
HF0961 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners notion and millinery bags.Advantag..
Film Tensile Strength at Break, TD 44.1 MPa
6400 psi
ASTM D882
Westlake Mxsten CV77516 Polyethylene Plastomer
Mxsten CV Plastomer CV77516 resin is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a very low se..
Film Tensile Strength at Break, TD 44.1 MPa
6400 psi
ASTM D882
ExxonMobil Exceed™ 1327KD Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327KD is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327KD is fully formula..
Film Tensile Strength at Break, TD 44.1 MPa
6400 psi
ASTM D882
ExxonMobil Exceed™ 2018KB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 2018KB is a metallocene catalyzed ethylene-hexene copolymer. Films made from Exceed 2018KB have outstanding tensile, impact strength, and puncture. These superior strengt..
Film Tensile Strength at Break, TD 44.1 MPa
6400 psi
Ultimate; ASTM D882
LG Chemical SEETEC SF316 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Additives- Medium slip agent, Medium antiblocking agentApplications: Agricultural & i..