Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 44.7 MPa
6480 psi
ASTM D882
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP)
AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi..