Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 45.26 MPa | 6565 psi | ASTM D882 |
Dow ATTANE™ 4201G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |