Polymer Property : Film Tensile Strength at Break, TD = 4860 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 33.5 MPa
4860 psi
Calculated from mfr's report of 17 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® N196 Paper, 2 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..