Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
3 mil; ASTM D882
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin
Features: Moderate toughness and strengthGood stiffnessEasy processabilityExcellent seal properties Applications: Heavy duty shipping sacks requiring moderate toughness and high stiffnessIndustrial ..
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
ExxonMobil Escorene® LD 701.ID Blown Film Resin
Escorene Ultra LD 701.ID is a fraction melt index, 10.5 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particularly..
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
ExxonMobil LL 1001x26 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. ..