Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 10.0 - 53.9 MPa
1450 - 7820 psi
Average value: 18.9 MPa Grade Count:31
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..