Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 55.9 MPa

@Thickness 0.0250 mm
8110 psi

@Thickness 0.000984 in
ASTM D882
LG Chemical SEETEC PF150 HDPE
Features: Characteristics: Good impact & tear strength, High speed & superior heat sealing propertiesAdditives: Anti-oxidants, LubricantsApplication: Shopping bags, Thin films, Trash bags, Multiwall..