Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 40.7 MPa
5900 psi
ASTM D882
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, high antiblock, and processing aid additiveCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, can..
Film Tensile Strength at Break, TD 40.7 MPa
5900 psi
ASTM D882
DuPont™ Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1601 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Film Tensile Strength at Break, TD 40.7 MPa
5900 psi
ASTM D882
DuPont™ Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1601-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s..
Film Tensile Strength at Break, TD 40.7 MPa
5900 psi
ASTM D882
DuPont™ Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1601-2LM (Low Moisture) is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications:..
Film Tensile Strength at Break, TD 40.7 MPa
5900 psi
ASTM D882
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Film Tensile Strength at Break, TD 40.7 MPa
5900 psi
ASTM D882
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin
Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The..
Film Tensile Strength at Break, TD 40.7 MPa
5900 psi
ASTM D882
NOVA Chemicals Sclair® 11H1 LLDPE Film Resin  (discontinued **)
Low gel, Excellent heat sealability, Easy processability, High toughness and strengthApplications: Heavy duty sack, High strength packagingAdditives: Process stabilizer, Polymer process aid, Antiblo..