Polymer Property : Film Tensile Strength at Break, TD = 6540 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 45.1 MPa
6540 psi
ASTM D882
Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Film Tensile Strength at Break, TD 45.1 MPa
6540 psi
ASTM D882
Chevron Phillips Dynex™ D508A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Film Tensile Strength at Break, TD 45.1 MPa
6540 psi
ASTM D882
Dow DX5E66 Polypropylene Homopolymer Resin
OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P..