Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | >= 67.6 MPa | >= 9800 psi | ASTM D 882 A |
Total 2285 HDPE Bimodal Film Resin Applications: T-shirt sacks, trash can liners, merchandise bags, multi-wall liner, deli wrapInformation provided provided by Total Petrochemicals. |
|||
Film Tensile Strength at Break, TD | >= 67.6 MPa | >= 9800 psi | ASTM D 882 A |
Total 2287 HDPE Bimodal Film Resin Broad molecular weight distribution. Designed for die build-up sensitive equipmentApplications: T-shirt sacks, trash can liners, merchandise bags, deli wrapInformation provided provided by Total Pe.. |