Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 46.9 MPa
6800 psi
ASTM D882
LyondellBasell Alathon® L4907 High Density Polyethylene
ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro..
Film Tensile Strength at Break, TD 46.9 MPa
6800 psi
ASTM D882
ExxonMobil Exact™ 3040 Cast Ethylene-based Plastomer Resin
Product Description: Exact 3040 is an ethylene-based hexane copolymer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monolayer and coextrusion cast fi..
Film Tensile Strength at Break, TD 46.9 MPa
6800 psi
ASTM D882
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 0.6 mil Film, Stiff  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope..
Film Tensile Strength at Break, TD 46.9 MPa
6800 psi
ASTM D882
ExxonMobil Enable™ 35-05CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 35-05CH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..