Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 41.4 - 49.6 MPa | 6000 - 7200 psi | ASTM D882 |
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf.. |
|||
Film Tensile Strength at Break, TD | 41.4 - 49.6 MPa | 6000 - 7200 psi | ASTM D882 |
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |