Polymer Property : Film Tensile Strength at Break, TD = 73.84 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 73.84 MPa
10710 psi
ASTM D882
ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications
Product Description: Exact 3132 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3132 is designed for both monolayer and multilayer blo..