Polymer Property : Film Tensile Strength at Break, TD = 81.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 81.2 MPa
11800 psi
Calculated from mfr's report of 497 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® 410 Paper, 24 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Film Tensile Strength at Break, TD 81.2 MPa
11800 psi
Calculated from mfr's report of 524 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® 410 Paper, 25.5 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..