Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 56.0 MPa | 8120 psi | ASTM D882 |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Film Tensile Strength at Break, TD | 56.0 MPa | 8120 psi | ASTM D882 |
SABIC FJ00952 High Density Polyethylene for Blown Film Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, .. |
|||
Film Tensile Strength at Break, TD | 56.0 MPa | 8120 psi | ASTM D882 |
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b.. |
|||
Film Tensile Strength at Break, TD | 56.0 MPa | 8120 psi | ASTM D882 |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Film Tensile Strength at Break, TD | 56.0 MPa | 8120 psi | ISO 527-3 |
Total HDPE HL 717 High Density Polyethylene - Blown Film HDPE HL 717 is a high density polyethylene produced by the gas phase polymerization process with hexene as a comonomer.HDPE HL 717 is a monomodal HDPE with a broad molecular weight distribution. It.. |
|||
Film Tensile Strength at Break, TD | 56.0 MPa | 8120 psi | ASTM D882 |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Film Tensile Strength at Break, TD | 56.0 MPa | 8120 psi | ASTM D882 |
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom.. |