Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 96.5 - 117 MPa
14000 - 17000 psi
ASTM D882
Honeywell Capran® Unidraw (1.00 mil) Nylon 6 Film  (discontinued **)
Description: Capran® Unidraw is a 1.00 mil (25 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str..
Film Tensile Strength at Break, TD 96.5 MPa
14000 psi
ASTM D882
Honeywell Capran® NyLid™ OMBS-100M Nylon Lidding Film  (discontinued **)
Description: Capran® NyLid™ OMBS-100M is a mono-axially oriented, co-extruded Nylon 6/EVOH/Nylong 6 clear film with a print/lamination receptive coating having excellent gas barrier through a broa..
Film Tensile Strength at Break, TD 96.5 MPa
14000 psi
ASTM D882
Dow Saran® 560 Clear Plastic Barrier Film
Saran™ 560 is a clear biaxially oriented monolayer barrier film, designed for unit packaging and other applications. It is available in 6 gauge.Information provided by Dow