Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 68.3 MPa
9900 psi
ASTM D882
ExxonMobil Exceed™ 1018CA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018 CA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018CA have outstanding tensile, puncture resistance and very good sealing properties. These..