Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 0.945 - 70.3 MPa | 137 - 10200 psi | Average value: 9.53 MPa Grade Count:10 |
Overview of materials for Polycarbonate-Urethane This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr.. |