Mechanical Properties Metric English Comments
Flexural Yield Strength 700 MPa
102000 psi
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, E-glass Balanced fabric 390 g/m2
Information provided by HexCel
Flexural Yield Strength 700 MPa
102000 psi
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, E-glass Balanced Fabric 300 g/m2
Information provided by HexCel