Polymer Property : Flexural Yield Strength = 10670 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 73.55 MPa

@Thickness 6.40 mm
10670 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
Flexural Yield Strength 73.55 MPa

@Thickness 6.40 mm
10670 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali