Polymer Property : Flexural Yield Strength = 112.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 112.8 MPa
16360 psi
ASTM D790
Samsung Cheil Industries Starex® HF-5330S ASA, Unreinforced  (discontinued **)
Amorphous Styrene Acrylonitrile (SAN)Characteristics: Heat Resistant: Impact and Chemical Resistance, Surface GlossApplications: Oil Filter Case, Lubricant Can, Refrigerator and Hair Dryer Component..