Polymer Property : Flexural Yield Strength = 11288 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 77.828 MPa
11288 psi
ASTM D790
KKPC Kuhmo GP 125EB Extrusion Molding GPPS
Key features: PSP Common Uses: Fruit, egg cell.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability of dimension.Da..