Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 124.1 MPa | 18000 psi | ASTM D790 |
PTS Trimid® N66-100HL Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 124.1 MPa | 18000 psi | ASTM D790 |
PTS Trimid® N66-100NL Nucleated, Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 124.1 MPa | 18000 psi | |
Abatron AboCast/AboCure 8109-8 All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi.. |