Polymer Property : Flexural Yield Strength = 130 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 90.0 - 130 MPa

@Temperature 80.0 - 80.0 °C
13100 - 18900 psi

@Temperature 176 - 176 °F
Average value: 121 MPa Grade Count:9
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..