Mechanical Properties Metric English Comments
Flexural Yield Strength 91.56 MPa
13280 psi
ASTM D790
KKPC Kuhmo GP 125BL Extrusion Molding GPPS
Key features: PSP Common Uses: Sheeting, instant noodle cups.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability o..