Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 7.60 - 134 MPa | 1100 - 19400 psi | Average value: 84.2 MPa Grade Count:76 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Yield Strength | 82.7 - 134 MPa | 12000 - 19500 psi | Average value: 102 MPa Grade Count:7 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |