Polymer Property : Flexural Yield Strength = 1570 MPa
Polymer Property :
Flexural Yield Strength =
1570 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Yield Strength
1570
MPa
228000
psi
Hexcel® HexPly® EH04 Epoxy Resin System, M35J Fiber
MS35J 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel