Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 164.6 MPa
23870 psi
ASTM D790
Plenco 51335 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51335 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in black only.Information ..