Polymer Property : Flexural Yield Strength = 17.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 17.8 MPa
2590 psi
ASTM D790
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic
SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo..