Polymer Property : Flexural Yield Strength = 19100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 86.2 - 132 MPa
12500 - 19100 psi
Average value: 105 MPa Grade Count:7
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum..