Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 143 MPa @Thickness 3.20 mm |
20800 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
Flexural Yield Strength | 143 MPa | 20800 psi | ASTM D790 |
LyondellBasell Hostacom™ PF062-3 Polypropylene Homopolymer Description: Hostacom™ PF062-3 high melt flow, 5,200 MPa flexural modulus, chemically coupled, 30% glass fiber-reinforced polypropylene homopolymer has good impact strength, high stiffness and very.. |